1(1737095541924).jpg
+
  • 1(1737095541924).jpg

TPV

Categories:

Thermoplastic Elastomers


Thermoplastic vulcanizate (TPV), which consists of a polyolefin phase (PP) with a dynamically cured EPDM phase, is closely dispersed in the PP matrix which gives rubber-like properties and has the advantage of thermoplastic processing techniques.
Get A Quote

Brief introduction:

Thermoplastic vulcanizate (TPV), which consists of a polyolefin phase (PP) with a dynamically cured EPDM phase, is closely dispersed in the PP matrix which gives rubber-like properties and has the advantage of thermoplastic processing techniques.

The final blend morphology always consists of cross-linked, micron sized elastomer particles dispersed in a polymer matrix.Because of the strong mechanical shearing and the chemical cross-linking by crosslinking agent, the rubber phase is cut into a large number of micron-scale cross-linked rubber particles dispersed in the thermoplastic resin matrix in the continuous phase thermoplastic resin matrix.

Benefits

  • Superior lightness
  • Rubber elasticity
  • Heat resistance
  • Cold resistance
  • Weatherability, Ozone resistance
  • Chemical resistance
  • Electrical insulation performance

 

Testing method

Unit

 

IC55A

IC65A

IC7A

IC85A

IC40D

IC50D

IC55A-01

IC65A-01

IC75A-01

Hardness  Shore A/D

ASTMD2240

55A

65A

75A

85A

40D

50D

55A

65A

75A

Density    g/cm3

ASTMD792

0.95

0.96

0.96

0.97

0.97

0.95

0.95

0.95

0.95

Tensilestressat 100% , MPa

ASTMD412

2.4

2.9

3.4

5.6

8.5

11.5

2.4

2.9

3.4

Tensile strength, MPa

ASTMD412

4.4

6.0

8.0

13.5

18.5

20

4.5

6.2

8.5

Elongation at break,%

ASTMD412

406

414

462

464

502

500

410

425

460

Tear strength, KN/m

ASTMD624

21.2

25.0

33.1

55.0

78.0

98

22.5

28.9

35.2

Compression set , 22h/70°C,%

ASTMD395

31.9

32.5

35.0

38.2

42.0

45.0

31.9

32.5

35.0

Brittle temperature, °C

ASTMD746

-60

-60

-60

-55

-50

-50

-60

-60

-60

Processing temperature, °C

170-190

Application :

Noted:

▲ Use PP or PE to clean the material before processing, and the raw material is dried at 90 ℃ -100 ℃ for 1.5 to 2 hours;

▲ Dye with PP or PE grade masterbatch, add at a rate of 2-3%;

▲ The processing temperature is between 165 ℃ and 200 ℃, and the highest temperature should not exceed 200 ℃;

▲ The length-diameter ratio of the equipment during extrusion processing should not be less than 25;

▲ Processing parameters such as temperature, pressure, and injection speed must be carefully adjusted during vertical injection.

Remarks: The above indicators are for reference. If there are special requirements on certain performances, Jinling Opt can customize it according to customer needs. For details, please contact us. Remarks: The above indicators are for reference. If there are special requirements on certain performances, our company can customize them individually according to customer needs. For details, please call us.

Key words:

Thermoplastic elastomers

Previous:

Next:

Online Message

* Note: Please be sure to fill in the information accurately and keep the communication unblocked, we will get in touch with you as soon as possible

%{tishi_zhanwei}%

Online Message

* Note: Please be sure to fill in the information accurately and keep the communication unblocked, we will get in touch with you as soon as possible

%{tishi_zhanwei}%